http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2009239245-A
Outgoing Links
Predicate | Object |
---|---|
assignee | http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_9df90d7822cc480ce12c480f4089e229 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/H01L41-113 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C04B35-491 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C04B35-49 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/H01L41-39 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/H01L41-257 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/H01L41-187 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/H01L41-22 |
filingDate | 2008-08-01-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor | http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_f3052cccd203ba4c106aa744e6b04f96 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_73d1b0976ede6aebec01daeabed56005 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_d7c83359d142498fed17039a1d097201 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_a59f222f2f5ac036daf9da54ea5565d7 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_e71138b737e9b356b565de6d507019d8 |
publicationDate | 2009-10-15-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | JP-2009239245-A |
titleOfInvention | Piezoelectric material |
abstract | Provided is a piezoelectric body in which an appropriate amount of an appropriate additive is added to improve a power generation amount per unit volume. In a piezoelectric element structure, 1 is a piezoelectric body manufactured by adding 1 mol% of niobium as an additive, and applying a polarization electric field of 1.5 kV / mm in the process of polarization, 2 is an electrode, 3 , 4 are output terminals. Electrodes 2 are formed on the upper and lower surfaces of the piezoelectric body 1 to constitute a piezoelectric element, and the electrodes 2 of the stacked piezoelectric elements are connected with the same polarity to form output terminals 3 and 4. As a base material of the piezoelectric body, lead zirconate titanate (PZT) which is a piezoelectric power generator is preferable. As an additive to be added to the base material in an amount of 0.1 to 4 mol%, it is introduced into the B site having a perovskite crystal structure such as niobium, tungsten, tantalum, lanthanum, antimony, bismuth, and thorium oxide, and has a low elastic modulus. An element that can supply a donor to a base material as an element is preferable. [Selection] Figure 5 |
isCitedBy | http://rdf.ncbi.nlm.nih.gov/pubchem/patent/WO-2012057221-A1 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2012109552-A http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-8669695-B2 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/CN-102163689-B http://rdf.ncbi.nlm.nih.gov/pubchem/patent/CN-102163689-A |
priorityDate | 2007-10-17-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type | http://data.epo.org/linked-data/def/patent/Publication |
Incoming Links
Total number of triples: 52.