http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2009221402-A
Outgoing Links
Predicate | Object |
---|---|
assignee | http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_d93502a23a72b56472bc75854cfe7c60 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08G61-08 |
filingDate | 2008-03-18-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor | http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_fa80477d7468de0e6829537852655f00 |
publicationDate | 2009-10-01-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | JP-2009221402-A |
titleOfInvention | Norbornene monomer ring-opening polymerization catalyst system, and ring-opening polymer and method for producing ring-opening polymer hydride |
abstract | Provided is a ring-opening polymerization catalyst system capable of obtaining a norbornene-based ring-opening polymer excellent in filtration performance and a hydride thereof at a relatively low cost by improving a ring-opening polymerization method of a norbornene-based monomer. To do. A ring-opening polymerization catalyst system of a norbornene monomer comprising a combination of (a) a tungsten compound, (b) an organoaluminum compound, (c) a secondary alcohol, and (d) a tertiary alcohol. The molar ratio (c / b) of the secondary alcohol to the organoaluminum compound is 0.90 to 1.15, and the molar ratio (d / b) of the tertiary alcohol to the organoaluminum compound is A ring-opening polymerization catalyst system of a norbornene-based monomer within a range of 0.01 to 0.11. [Selection figure] None |
isCitedBy | http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2013075976-A http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-11066497-B2 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/WO-2014103830-A1 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-11597797-B2 |
priorityDate | 2008-03-18-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type | http://data.epo.org/linked-data/def/patent/Publication |
Incoming Links
Total number of triples: 200.