http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2009203366-A
Outgoing Links
Predicate | Object |
---|---|
assignee | http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_d9cb217f83556ce2a418344c2d485415 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08J9-28 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08J9-36 |
filingDate | 2008-02-28-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor | http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_ba08bed5da2ea50326658dd639eee961 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_f6444c760e62a868f676ecf9f51ebf3b |
publicationDate | 2009-09-10-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | JP-2009203366-A |
titleOfInvention | Polysiloxane-coated polyamide porous fine particles and method for producing the same |
abstract | PROBLEM TO BE SOLVED: To provide polyamide porous fine particles having a single particle-like powder without aggregation and having further improved functions for applications such as cosmetic raw materials, optical film applications in electronic fields, and coatings. A number-average particle diameter of 30μm from 1 [mu] m, the pores and the surface of the polyamide porous particle is a BET specific surface area of 0.1m 2 / g~80m 2 / g, the polyamide porous particle 1 A polysiloxane-coated polyamide porous fine particle coated with more than% by weight of polysiloxane and heat-treated at a temperature of less than 100 ° C. and a treatment method thereof. [Selection] Figure 3 |
priorityDate | 2008-02-28-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type | http://data.epo.org/linked-data/def/patent/Publication |