abstract |
【Task】 To provide a laminated film having excellent surface hardness and free from cracks during molding. [Solution] A laminated film in which a hard coat layer is provided on at least one surface of a base film, wherein the maximum value of the surface hardness of the hard coat layer in an ultra-micro hardness tester is 0.05 GPa or more and 4.0 GPa or less, and an atmosphere of 100 ° C. A laminated film having a lower crack elongation of 15% or more and less than 250%. [Selection figure] None |