http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2009179890-A
Outgoing Links
Predicate | Object |
---|---|
assignee | http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_50ff960bba3c8cfabd7f3141e0ff0189 http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_1374dd16777534b65ad4422333245af8 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08G73-08 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/D01F6-74 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/D02J13-00 |
filingDate | 2008-01-29-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor | http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_619c035fa142ee116df990453c9f21c1 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_63cc85630c4e22c13c7c5865e8950a69 |
publicationDate | 2009-08-13-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | JP-2009179890-A |
titleOfInvention | Manufacturing method of fiber molded body made of rigid heterocyclic polymer |
abstract | The present invention provides a method for producing a high molecular weight rigid heterocyclic polymer fiber molded body. A fiber molded body comprising a specific rigid heterocyclic polymer and having a specific viscosity of 5.0 to 15 dl / g measured at 25 ° C. with a methanesulfonic acid solution having a concentration of 0.03 g / 100 ml ( After obtaining I), it is heated at 100 to 250 ° C. for 1 to 50 hours, A method for producing a rigid heterocyclic polymer fiber molding (II) having a specific viscosity of 13 to 30 dl / g. [Selection figure] None |