Predicate |
Object |
assignee |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_bfe885803ddfc021f4f5ad13b5cc26b5 |
classificationCPCAdditional |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B29C2949-24 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B29C2949-22 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B29C2949-3024 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B29C2949-28 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B29C2949-26 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B29C2949-3032 |
classificationIPCAdditional |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B29L22-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B29K67-00 |
classificationIPCInventive |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B29C49-64 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B29C49-42 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B65D1-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08K9-04 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08L67-02 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08J5-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B29C49-08 |
filingDate |
2008-01-30-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_fb13951e2d7b3f102c4956262d984577 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_de4481256859f2dda71839332ecdf3fa |
publicationDate |
2009-08-13-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber |
JP-2009178891-A |
titleOfInvention |
Stretch blow molded container |
abstract |
An object of the present invention is to provide a stretch-molded container having excellent appearance characteristics such as transparency, excellent stretch moldability, and excellent stretch balance such as thickness and shape uniformity. A stretch blow molded container formed from a resin composition comprising an ethylene terephthalate-based polyester resin and dry hydrophobic silica particles whose surface is covered with a hydrophobic organic functional group. δT (° C.) = TC1 (2nd) −TC1 (1st) In the formula, TC1 (1st) is the crystallization exothermic peak temperature of the unstretched portion of the container by a differential scanning calorimeter (DSC), and TC1 (2nd) is a differential scanning calorimeter (after melting and quenching the unstretched portion of the container) DSC) is characterized in that the value of δT (° C.) represented by crystallization exothermic peak temperature is greater than 0 and 14 or less. [Selection figure] None |
priorityDate |
2008-01-30-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type |
http://data.epo.org/linked-data/def/patent/Publication |