http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2009173705-A
Outgoing Links
Predicate | Object |
---|---|
assignee | http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_f09378c018e7719f171f7e91f2dd60fd |
classificationIPCAdditional | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B65D8-04 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C09J167-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C09J11-06 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C09J11-04 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C09J155-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C09J133-00 |
filingDate | 2008-01-22-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor | http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_d0269d63ac6874e3f378ff5c516a224d http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_ac459c77c8bf5f0f0b2862e6fb89dea4 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_a56a8b779282cc485278211feb7d10f5 |
publicationDate | 2009-08-06-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | JP-2009173705-A |
titleOfInvention | Metal can outer surface adhesive and polyester film bonded metal plate |
abstract | PROBLEM TO BE SOLVED: To provide an adhesive for outer surface of metal can excellent in blocking resistance used for production of a polyester film-bonded metal plate, and a polyester film-bonded metal plate using the adhesive. [Solution] For 100 parts by mass of the polyester resin (A) having a number average molecular weight of 5,000 to 60,000 and a glass transition temperature of 30 to 80 ° C., 0.1 to 30 parts by mass of the crosslinking agent (B), the following characteristics A metal can outer surface adhesive containing 0.3 to 10 parts by mass of acrylic resin (C). Acrylic resin (C): at least one monomer (c1) 5 to 95 selected from isobornyl acrylate, isobornyl methacrylate, 2-ethylhexyl acrylate and 2-ethylhexyl methacrylate, based on the total mass part of the constituent monomers It is formed by copolymerizing a monomer component consisting of 5 parts by mass, 5 to 30 parts by mass of a hydroxyl group-containing polymerizable unsaturated monomer (c2) and 0 to 90 parts by mass of another polymerizable unsaturated monomer (c3). [Selection figure] None |
isCitedBy | http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2019001944-A http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2013086413-A http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2011184602-A http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2018529807-A http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2016003273-A |
priorityDate | 2008-01-22-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type | http://data.epo.org/linked-data/def/patent/Publication |
Incoming Links
Total number of triples: 41.