http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2009167346-A
Outgoing Links
Predicate | Object |
---|---|
assignee | http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_efbfdc7316d3b1b7ceaee5366a61b6e0 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C09J4-02 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C09J109-00 |
filingDate | 2008-01-18-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor | http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_56e0be8ccdab294751f07d564f9df842 |
publicationDate | 2009-07-30-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | JP-2009167346-A |
titleOfInvention | Storage stabilization method of active energy ray cross-linking adhesive |
abstract | The present invention provides a novel storage stabilization method for an adhesive having high adhesive strength, excellent compatibility of components constituting the adhesive, and greatly improved storage stability of the adhesive. (A) A conjugated diene oligomer having a weight average molecular weight of 500 to 100,000 having at least one functional group having a (meth) acryloyl group at its terminal, and (B) a general formula (100) I) 50 active energy ray polymerizable compounds containing a polymerizable compound (meth) acrylic monomer having a structure represented by the formula (5) to 500 parts by mass and (C) a specific alkanediol (meth) diacrylate. It is included at a ratio of ˜1000 parts by mass. [Selection figure] None |
isCitedBy | http://rdf.ncbi.nlm.nih.gov/pubchem/patent/KR-20180032040-A http://rdf.ncbi.nlm.nih.gov/pubchem/patent/KR-20180034973-A http://rdf.ncbi.nlm.nih.gov/pubchem/patent/TW-I735664-B http://rdf.ncbi.nlm.nih.gov/pubchem/patent/KR-102487396-B1 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/WO-2018062744-A1 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/KR-102143802-B1 |
priorityDate | 2008-01-18-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type | http://data.epo.org/linked-data/def/patent/Publication |
Incoming Links
Total number of triples: 193.