http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2009157304-A
Outgoing Links
Predicate | Object |
---|---|
assignee | http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_73ebc284a55d5daf0e209d6186c9e65c |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/G02B1-11 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/G02B1-10 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/G02B3-00 |
filingDate | 2007-12-28-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor | http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_7bf840b3819d13a262ca576027d4ef76 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_2b915343103a28cc99a038c7a0643efa |
publicationDate | 2009-07-16-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | JP-2009157304-A |
titleOfInvention | Lens and lens manufacturing method |
abstract | A lens having high adhesion between a hard coat layer and an antireflection layer and a method for producing the same are provided. A lens substrate 11, a hard coat layer 12 formed on the lens substrate 11, an antireflection layer 14 formed on the hard coat layer 12, a hard coat layer 12, and an antireflection layer 14 are provided. The lens 1 is provided with an adhesive layer 13 provided between the two, and the adhesive layer 13 has the same or substantially the same refractive index as that of the hard coat layer 12. The thickness of the adhesion layer 13 is preferably 0.5 μm or more and 5 μm or less. Moreover, it is preferable that the contact | adherence layer 13 is formed from the composition containing 5 mass% or more and 20 mass% or less of silica sol by solid content weight ratio. [Selection] Figure 1 |
priorityDate | 2007-12-28-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type | http://data.epo.org/linked-data/def/patent/Publication |
Incoming Links
Total number of triples: 121.