http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2009150586-A
Outgoing Links
Predicate | Object |
---|---|
assignee | http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_283a2b2a3dad59382bb9ab870324effb |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C23C28-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B32B15-08 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B01J21-06 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B01J35-02 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/F28F1-12 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/F28F13-18 |
filingDate | 2007-12-19-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor | http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_68f58fd63c2f645aca478548947f120c http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_7cce290ad92974019ba55b400a311d1e |
publicationDate | 2009-07-09-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | JP-2009150586-A |
titleOfInvention | Fins for heat exchanger |
abstract | An object of the present invention is to provide hydrophilicity from the initial stage of use where light irradiation is started without adversely affecting the mold during molding such as press working, and excellent hydrophilicity by irradiating light. Providing a fin material for a heat exchanger capable of maintaining the temperature for a long time. A base material 2 made of aluminum or an aluminum alloy, a base layer 3 formed on the surface of the base material 2, a photocatalyst layer 4 formed on the base layer 3, and a photocatalyst layer 4 are formed. This is a heat exchanger fin material 1 comprising a hydrophilic resin layer 5. The photocatalyst layer 4 is formed by dispersing photocatalyst particles 42 in a base resin 41. The hydrophilic resin layer 5 has a thickness of more than 0.5 μm and not more than 3 μm. The fin material 1 for heat exchanger is placed in a container in which pure water is overflowed at a rate of 1 L / min without irradiating light having a wavelength capable of exciting the photocatalyst particles 42 with a test piece having a length of 50 mm and a width of 50 mm. The contact angle with water is 40 ° or less before and after the running water test immersed for 10 minutes. [Selection] Figure 1 |
isCitedBy | http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2012215347-A http://rdf.ncbi.nlm.nih.gov/pubchem/patent/WO-2023282112-A1 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/WO-2023282111-A1 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/EP-2211438-A1 |
priorityDate | 2007-12-19-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type | http://data.epo.org/linked-data/def/patent/Publication |
Incoming Links
Total number of triples: 55.