Predicate |
Object |
assignee |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_fcc0b66123940d1b32783569ebfa2d45 |
classificationCPCInventive |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B32B27-08 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B32B27-28 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B32B7-12 |
classificationIPCAdditional |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B29K45-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B29L7-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B29L9-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B29L11-00 |
classificationIPCInventive |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08J7-04 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B32B27-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B29C48-305 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B05D5-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B05D7-04 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B29C55-02 |
filingDate |
2008-11-12-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_39242a29b03028d9d6c2669dbbb7da44 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_76976ef4f1eb2292145e6a87faa8463d http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_c0064a4f19bfb74f7dadf7ce84c713ff http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_bdde3357faaf11be2a38c820efb6896b http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_d611cbf7ad46903c012cb02bbf03b931 |
publicationDate |
2009-06-25-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber |
JP-2009137290-A |
titleOfInvention |
Norbornene resin film having hard coat layer and method for producing norbornene resin film having hard coat layer |
abstract |
[PROBLEMS] To produce a norbornene resin film having a hard coat layer, which has a hard coat layer having excellent optical properties and sufficient surface hardness, and which can be obtained by a simple method. A method and a norbornene-based resin film having a hard coat layer are provided. There are provided a step of forming a norbornene-based resin base film and a step of forming a hard coat layer having at least two kinds of organic components on the obtained norbornene-based resin base film. The manufacturing method of the norbornene-type resin film which has a hard-coat layer in which the coat layer is phase-separated, and the norbornene-type resin film which has a hard-coat layer. [Selection figure] None |
isCitedBy |
http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-7127745-B2 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/WO-2021025055-A1 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-WO2021025055-A1 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2015061754-A |
priorityDate |
2007-11-15-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type |
http://data.epo.org/linked-data/def/patent/Publication |