http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2009137153-A
Outgoing Links
Predicate | Object |
---|---|
assignee | http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_3cefaf7862fb1d052972f5acebe72a43 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C23C18-18 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C23C28-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C23C18-20 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B32B15-01 |
filingDate | 2007-12-06-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor | http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_a6ecf5b61a64204097e236485d60a9d9 |
publicationDate | 2009-06-25-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | JP-2009137153-A |
titleOfInvention | Precious metal coatings, jewelry and ornaments, apparel products, electronic equipment products using the same and methods for producing them |
abstract | PROBLEM TO BE SOLVED: To deposit a noble metal directly on the surface of a base material or to deposit the precious metal film on the base material surface, so that the adhesion of the film depends mainly on the anchor effect on the surface of the base material. There was a big problem that the peelability was bad. The present invention provides a noble metal coating characterized in that it is formed on a substrate surface through a lower layer coating made of at least an alkoxysilyl group-containing triazine thiol compound or a thiol compound. [Selection] Figure 1 |
isCitedBy | http://rdf.ncbi.nlm.nih.gov/pubchem/patent/WO-2012046651-A1 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-8753748-B2 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-9593423-B2 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-4936344-B1 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2018037639-A |
priorityDate | 2007-12-06-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type | http://data.epo.org/linked-data/def/patent/Publication |
Incoming Links
Total number of triples: 28.