http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2009079105-A
Outgoing Links
Predicate | Object |
---|---|
assignee | http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_4a661794c0862547d70b8a76f0c163dc |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C09D4-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C09D133-14 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C09D7-12 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C09D5-44 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C25D13-06 |
filingDate | 2007-09-26-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor | http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_46da129e5388823c223a33369b879eb7 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_4e791936842039b20a57ec2c8ec25cc8 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_ee7571174216217af29eaf08cc681d9f |
publicationDate | 2009-04-16-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | JP-2009079105-A |
titleOfInvention | Composition for UV-curable cationic electrodeposition coating and coating film thereof |
abstract | The present invention provides an ultraviolet curable cationic electrodeposition coating composition having good liquid temporal stability, high sensitivity, and excellent surface curability, adhesion, corrosion resistance, weather resistance, and chemical resistance. . (A) A water-soluble or water-dispersible vinyl copolymer having an unsaturated group at the end of a main chain obtained by copolymerization using the following components (a) to (c): 50-80 parts by weight, (A) Copolymerizable vinyl monomer having a tertiary aminoalkyl group as a substituent 4 to 15 parts by weight (b) Copolymerizable vinyl monomer other than (a) 85 to 96 parts by weight (c) Addition-cleavage type chain transfer agent 0.05 to 20 parts by weight (B) 3 or more unsaturated groups per molecule with respect to 100 parts by weight of the total copolymerizable vinyl monomers (a) and (b) 20 to 50 parts by weight of a compound having (C) Light having a dissolution amount at 25 ° C. in 100 g of water containing 3% of an alcohol solvent of less than 0.02 g and a molar absorption coefficient ε of maximum absorption at 200 nm to 400 nm of 10,000 L / mol · cm or more. The composition for ultraviolet curable cationic electrodeposition coatings containing 0.1-8 weight part with respect to a total of 100 weight part of a polymerization initiator (A) and (B). [Selection figure] None |
isCitedBy | http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2010083933-A |
priorityDate | 2007-09-26-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type | http://data.epo.org/linked-data/def/patent/Publication |
Incoming Links