http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2009074016-A
Outgoing Links
Predicate | Object |
---|---|
assignee | http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_252d8144b3f00a4a8d2dcdf7169ef1c8 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C09D5-24 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/D06M15-568 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C09K3-16 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C09D151-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/D06M15-27 |
filingDate | 2007-09-21-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor | http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_a9a2dfc76de54b8bb0a5dab15c5f5a00 |
publicationDate | 2009-04-09-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | JP-2009074016-A |
titleOfInvention | Durable antistatic agent and processing method thereof |
abstract | Disclosed is a durable antistatic agent for synthetic fibers which can be easily processed by a general processing machine, has little feel hardening by treatment, and has excellent durability and antistatic properties. In the presence of a block-type urethane prepolymer containing an ethylene oxide chain, (a) (meth) acrylic acid polyethylene glycol monomer or (meth) acrylic acid alkoxy polyethylene glycol monomer (25-100% by weight), (B) Synthetic fibers obtained by polymerizing a monomer mixture comprising 0 to 75% by weight of other copolymerizable ethylenically unsaturated monomers (where (a) + (b) = 100% by weight) Durable antistatic agent for use. [Selection figure] None |
isCitedBy | http://rdf.ncbi.nlm.nih.gov/pubchem/patent/CN-114875673-A |
priorityDate | 2007-09-21-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type | http://data.epo.org/linked-data/def/patent/Publication |
Incoming Links
Total number of triples: 77.