http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2009067854-A
Outgoing Links
Predicate | Object |
---|---|
assignee | http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_dc45703f67bc72a6db582867886fd5d5 http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_0ddb9f3656270bc5410be3679322fead |
classificationCPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B29B7-002 |
classificationIPCAdditional | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B29L31-58 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08F297-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08J3-12 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08L53-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08K3-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B29C41-18 |
filingDate | 2007-09-11-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor | http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_f3dac7d0717868d438188f6c45ef7875 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_b7b62ed0c8abf72fdda53a5205ccc4f8 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_34dbfa7bb9dad8bec2d4af0a41e28d96 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_72fb16b191004ecf8c7612e1b2845961 |
publicationDate | 2009-04-02-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | JP-2009067854-A |
titleOfInvention | Powder for skin molding for automobile interior and production method thereof |
abstract | [PROBLEMS] To provide a powder having good melt fluidity, excellent powder fluidity, and safe, weather resistance, flexibility, rubber elasticity, low temperature characteristics, adhesion to a polar resin, texture, appearance and the like. A manufacturing method is provided. A dispersion (Y) containing a thermoplastic elastomer composition (X) having a predetermined component, water (D), and a polyvinyl alcohol-based dispersant (E) is mixed with power per unit volume of the liquid. A process of heating up to a predetermined temperature while blowing steam while stirring with a pitched paddle blade under a condition where P / V is 0.2 kW / m 3 or more, and 5 minutes or more and 2 hours at 90 ° C. or more and less than 110 ° C. A powder is produced by a method including a step of producing a polymer spherical powder while removing the solvent (C) from the dispersion (Y) by less than steam stripping and a drying step. [Selection figure] None |
priorityDate | 2007-09-11-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type | http://data.epo.org/linked-data/def/patent/Publication |
Incoming Links
Total number of triples: 220.