Predicate |
Object |
assignee |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_88fbcd2a70a3c49d0aed69a000d55909 |
classificationIPCInventive |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B32B27-32 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B32B27-28 |
filingDate |
2007-08-31-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_8c80b887e1f545b398ff9313fa10c71a http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_224d1d6bf062fc47a572924e7815669c http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_055767897a3a31d74905c1ab156b7664 |
publicationDate |
2009-03-19-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber |
JP-2009056708-A |
titleOfInvention |
Laminate manufacturing method and laminate obtained thereby |
abstract |
Provided is a method for manufacturing a laminate that can suppress discoloration of a recycle layer and suppress generation of phase separation foreign matter (eyes). A layer comprising (A) a saponified ethylene-vinyl acetate copolymer having an ethylene content of 10 to 60 mol% and (B) a saponified ethylene-vinyl acetate copolymer having an ethylene content of 70 mol% or more. And (C) a method for producing a laminate including a recycled layer obtained by melt-molding a recovered material of a laminate including a polyolefin-based resin layer as a raw material. Then, the content of (B) in the recovered material to be melt-molded is adjusted to 0.001 wt% or more and less than 0.3 wt% with respect to the total amount of (A) + (C). is there. [Selection figure] None |
isCitedBy |
http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-11020945-B2 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-10358550-B2 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-5665860-B2 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/WO-2015041135-A1 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/CN-102844185-A http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-9457545-B2 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-10589493-B2 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/WO-2011136287-A1 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/RU-2740829-C2 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2015083665-A |
priorityDate |
2007-08-31-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type |
http://data.epo.org/linked-data/def/patent/Publication |