http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2009046748-A
Outgoing Links
Predicate | Object |
---|---|
assignee | http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_b9d0c82c6254d5b4bec8c96e45c9db7b |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C25B3-13 |
filingDate | 2007-08-22-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor | http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_e03930026532983d36786164e2e45366 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_f3ba588322aee3f318dcf79f04680047 |
publicationDate | 2009-03-05-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | JP-2009046748-A |
titleOfInvention | Cyano-bridged metal complex preparation method and cyano-bridge metal complex preparation apparatus |
abstract | To obtain a cyano-bridged metal complex having a uniform crystal orientation. An electrolytic cell (2) containing a solution containing alkali metal ions, transition metal ions, and cyano complex ions, a deposition electrode (3) disposed in the electrolytic cell (2), and A superposed voltage obtained by superimposing a DC voltage and an alternating voltage that periodically changes with a predetermined amplitude is applied to the electrode for precipitation (3), and cyano aligned in a predetermined crystal orientation on the electrode for precipitation (3) by electrolysis. A power supply device (6) for depositing a cross-linked metal complex, and a cyano cross-linked metal complex preparation device (1). [Selection] Figure 1 |
isCitedBy | http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2011208217-A |
priorityDate | 2007-08-22-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type | http://data.epo.org/linked-data/def/patent/Publication |
Incoming Links
Total number of triples: 25.