http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2009036850-A
Outgoing Links
Predicate | Object |
---|---|
assignee | http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_8fb9f44db08d1c42a53f3d28eaae416f |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/G03G9-087 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/G03G9-08 |
filingDate | 2007-07-31-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor | http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_415d37f207441623ed3c226fc506f9cd http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_eeab388560eb25f3405c3a0d21553b3a |
publicationDate | 2009-02-19-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | JP-2009036850-A |
titleOfInvention | Toner for electrophotography |
abstract | Disclosed is an electrophotographic toner that has excellent fixability and high-temperature offset resistance, and that suppresses fixing roller filming due to long-term printing durability. An electrophotographic toner obtained by externally adding an external additive to a toner base particle containing a binder resin, a release agent, and a colorant, wherein the binder resin comprises a polyester resin. The mold release agent contains a polypropylene wax having a melting point of 110 to 140 ° C. and a paraffin wax having a melting point of 70 to 90 ° C., and the average melting point of the release agent is 90 to 110 ° C. The toner for electrophotography, wherein the external additive contains melamine resin fine particles having an average particle size of 0.09 to 0.8 μm. [Selection figure] None |
isCitedBy | http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2011095413-A |
priorityDate | 2007-07-31-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type | http://data.epo.org/linked-data/def/patent/Publication |
Incoming Links
Total number of triples: 81.