http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2009029953-A
Outgoing Links
Predicate | Object |
---|---|
assignee | http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_132721b781afede2175d04e894580568 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08F2-16 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08F2-44 |
filingDate | 2007-07-27-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor | http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_65100befbb9e9f26d767219dd9ba3777 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_14c56c06349fb59a127690b8e66f786a http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_cc7e77399633c26d473ace551ad3712a |
publicationDate | 2009-02-12-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | JP-2009029953-A |
titleOfInvention | Method for producing vinyl resin particles |
abstract | Provided is a method for efficiently producing vinyl resin particles having wrinkles on a surface in an industrially advantageous manner. (A) An aqueous dispersion preparation step of preparing an aqueous dispersion by dispersing droplets of a vinyl monomer A containing a plasticizer comprising a fatty acid ester in an aqueous medium, and (b) A method for producing vinyl resin particles having an average particle diameter of 1 to 200 μm having wrinkles on the surface, including a polymerization step of polymerizing the vinyl monomer A in the aqueous dispersion, wherein in the step (b), A hydrocarbon compound having a solubility parameter of 13.0 to 15.0 (MPa) 1/2 is added to the polymerization reaction system in a state where the polymerization conversion of the vinyl monomer A is 50 to 80%. To do. [Selection] Figure 1 |
isCitedBy | http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2009029951-A http://rdf.ncbi.nlm.nih.gov/pubchem/patent/CN-114524896-A |
priorityDate | 2007-07-27-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type | http://data.epo.org/linked-data/def/patent/Publication |
Incoming Links
Total number of triples: 140.