http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2009007507-A
Outgoing Links
Predicate | Object |
---|---|
assignee | http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_d9cb217f83556ce2a418344c2d485415 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08F36-06 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08F2-01 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08F295-00 |
filingDate | 2007-06-29-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor | http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_10649198fd30a154b92f4b40e1047935 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_ee9f2e2a0dc2cf35cd85ebe73ea0c357 |
publicationDate | 2009-01-15-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | JP-2009007507-A |
titleOfInvention | Reinforced polybutadiene and method for producing the same |
abstract | PROBLEM TO BE SOLVED: To provide a reinforced polybutadiene rubber having a further enhanced reinforcing effect by syndiotactic 1,2-polybutadiene and a method for producing the same. SOLUTION: 1,3-Butadiene is cis-1,4 polymerized, followed by stirring parameters nd (2/3) (n: stirring speed (rpm), d: effective stirring radius (m)) of 35 or more, A reinforced polybutadiene rubber obtained in a process of syndiotactic 1,2 polymerization in which the relationship between the effective stirring diameter d (m) and the reaction vessel diameter D (m) is d / D ≧ 0.5, and a method for producing the same. [Selection figure] None |