http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2008534717-A
Outgoing Links
Predicate | Object |
---|---|
classificationCPCAdditional | http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08L2666-04 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08L31-04 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08L29-04 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08L3-02 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08L2666-02 |
classificationCPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C09J151-02 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08F285-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C09J103-02 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C09D151-02 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C09J103-04 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08F290-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08F251-02 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08F251-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08L51-02 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C09J103-08 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C09J129-04 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B27D1-10 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C09J133-02 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C09J131-04 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C09J5-04 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C09J103-10 |
filingDate | 2005-11-18-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationDate | 2008-08-28-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | JP-2008534717-A |
titleOfInvention | Method of adhering woodwork or decoration using a polymeric binder as a binder |
abstract | The present invention is a method of adhering a woodwork product or a decorative product using a polymerization binder as a binder. Polymeric binders include starch and polymerized polymeric materials. The method of making the binder is as follows: First, the starch and polymerized polymer are modified. Next, the modified starch and the polymerized polymer are put in a container having a temperature of 20 ° to 100 ° C. and subjected to branch polymerization to produce a polymerization binder. The present invention can bond all wood-based products. For example, wooden furniture, cloth furniture, kitchen furniture, veneer board, fine woodwork board, density board, decorative plywood. Products bonded using the binder of the present invention will not submerge when immersed for 48 hours. And even if it is boiled in hot water of 63 ° C for 3 hours, it will not tear. The standard sample cutting strength can reach a dry strength of 5-14 mpa and a wet strength of 2-7 mpa. It can also be used for interior wall paint, putty, interior wall tile, wallpaper, wall cloth, decorative paper, carpet, and leather. |
priorityDate | 2005-03-31-04:00^^<http://www.w3.org/2001/XMLSchema#date> |