http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2008532210-A
Outgoing Links
Predicate | Object |
---|---|
classificationCPCAdditional | http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08L83-04 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08L2203-202 |
classificationCPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08L23-04 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08L23-0869 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/H01B7-295 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08L21-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08L83-04 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/H01B3-441 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08K3-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/H01B11-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/H01B7-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08L23-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/H01B13-14 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/H01B9-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/H01B13-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/H01B7-295 |
filingDate | 2006-02-22-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationDate | 2008-08-14-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | JP-2008532210-A |
titleOfInvention | Power or communication cable with flame retardant polymer layer |
abstract | The invention in a first embodiment is a conduit or automobile wire consisting of an inner conductor core surrounded by a flame retardant layer made from a polymer composition in a continuous process, wherein the composition comprises (A) Olefin Homo and / or Copolymer (B) Silicone Group-Containing Compound, and (C) Inorganic Filler, MFR 2 of Component (A) Measured at a Load of 2.16 kg and at a Temperature of 190 ° C., and a Load of 2 . Concerning conduits or automotive wires, the ratio of the composition to MFR 2 measured below 16 kg and at a temperature of 190 ° C. is greater than 3.5 and the wires have a length of at least 100 m. In a second embodiment, the present invention is a power or communication cable or wire comprising a flame retardant layer made from a polymer composition, the composition comprising (A) an olefin homo and / or MFR 2 of component (A) measured under a load of 2.16 kg and at a temperature of 190 ° C., comprising a copolymer (B) a silicone group-containing compound and (C) an inorganic filler, and under a load of 2.16 kg and a temperature of 190 It relates to a power or communication cable or wire, wherein the ratio of the composition measured at 0 ° C. to MFR 2 is greater than 3.5, and the cable or wire further comprises at least one further layer. [Selection figure] None |
isCitedBy | http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2014125575-A http://rdf.ncbi.nlm.nih.gov/pubchem/patent/WO-2014103904-A1 |
priorityDate | 2005-02-23-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type | http://data.epo.org/linked-data/def/patent/Publication |