Predicate |
Object |
classificationCPCAdditional |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/D21H23-04 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/D21H17-44 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/D21H17-28 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/D21H21-16 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/D21H21-24 |
classificationCPCInventive |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/D21H17-44 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/D21H17-16 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/D21H21-26 |
classificationIPCInventive |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/D21H17-44 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/D21H17-15 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/D21H21-16 |
filingDate |
2005-10-27-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationDate |
2008-08-14-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber |
JP-2008531864-A |
titleOfInvention |
Low shear cellulose reactive sizing agent for wet end application |
abstract |
The present invention includes (a) supplying a paper material system, (b) forming an aqueous size emulsion containing an alkenyl succinic anhydride component without applying high shear force, and (c) forming in step b. Subjecting the resulting emulsion to a post-dilution step in the presence of a cationic component under non-shearing conditions to produce a post-dilution emulsion having an improved size effect; and (d) a post-dilution emulsion Relates to a method for sizing a paper product comprising the steps of: adding to a paper stock and (e) forming a paper web. |
isCitedBy |
http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2007301532-A http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2017500454-A |
priorityDate |
2005-03-03-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type |
http://data.epo.org/linked-data/def/patent/Publication |