Predicate |
Object |
classificationCPCAdditional |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08J2323-10 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08J2323-12 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/Y02W30-62 |
classificationCPCInventive |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08J11-28 |
classificationIPCInventive |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08L23-10 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08K5-3477 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08K5-36 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08K5-3435 |
filingDate |
2005-08-31-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationDate |
2008-04-24-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber |
JP-2008512533-A |
titleOfInvention |
Degradation of polypropylene using hydroxylamine ester composition |
abstract |
Disclosed is a degradation of polypropylene using a hydroxylamine ester composition. The present invention relates to a novel composition comprising a hydroxylamine ester and a thio compound, said composition being suitable for reducing the molecular weight of polypropylene, propylene copolymers or polypropylene blends and consequently a temperature below 220 ° C. Provides excellent decomposition performance. [Selection figure] None |
isCitedBy |
http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2015024995-A http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2019518146-A http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2012521573-A http://rdf.ncbi.nlm.nih.gov/pubchem/patent/KR-20190015247-A http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-7003064-B2 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/KR-102348350-B1 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2009533505-A |
priorityDate |
2004-09-09-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type |
http://data.epo.org/linked-data/def/patent/Publication |