abstract |
PROBLEM TO BE SOLVED: To provide a thermoplastic olefin composition useful for producing a molded article having high surface glossiness and damage resistance. SOLUTION: (1) about 10 to 90 parts by weight of propylene homopolymer, copolymer or terpolymer, (2) olefin polymer composition comprising low molecular weight ethylene copolymer rubber, ethylene and C 3 -C 8 produced with metallocene catalyst about 90 to about 10 parts by weight of an elastomeric copolymer with α-olefin, or a mixture of the two, and (3) about 0.1 to about 10 parts by weight per 100 parts by weight of the lubricant (1) + (2) Use the composition. [Selection figure] None |