http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2008291237-A
Outgoing Links
Predicate | Object |
---|---|
assignee | http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_ad2cd796f8c4dcb425ddcc68707d3444 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08J5-18 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08G63-672 |
filingDate | 2008-04-23-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor | http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_07d29f5a1bcaa614d8558760f2023e25 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_8f8a6ab5c06f685ef0eb1fc4352a32a6 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_e4d4d376351d2141a5e7636a9ee40887 |
publicationDate | 2008-12-04-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | JP-2008291237-A |
titleOfInvention | Polyester elastomer composition and use thereof, and method for producing polyester elastomer composition |
abstract | PROBLEM TO BE SOLVED: To provide a polyester elastomer which is excellent in heat resistance, mechanical properties, color tone, and flavor retention and can be advantageously used as a container for food or beverage, packaging material or fiber. . In a polyester elastomer obtained from a dicarboxylic acid component mainly composed of an aromatic dicarboxylic acid, a glycol component mainly composed of 1,4-butanediol and having a molecular weight of less than 250, and a polyalkylene glycol having a molecular weight of 400 to 6000. 50 ppm or less of free aromatic dicarboxylic acid, 10 ppm or less of free butanediol, 10 ppm or less of free aromatic dicarboxylic acid monobutylene glycol ester, and 100 ppm or less of free aromatic dicarboxylic acid dibutylene glycol ester This can be solved by a polyester elastomer composition. [Selection figure] None |