http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2008285794-A
Outgoing Links
Predicate | Object |
---|---|
assignee | http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_1374dd16777534b65ad4422333245af8 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/D01F9-145 |
filingDate | 2007-05-21-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor | http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_a200d4c62c816de43f0bde4685ab359a http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_1af4b519a67e085f0cfdf817cc4ee56d http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_afff40d47fd6039b98e1aef662df9919 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_925f466a7e3ee934e47eb72295f87135 |
publicationDate | 2008-11-27-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | JP-2008285794-A |
titleOfInvention | Carbon fiber and method for producing the same |
abstract | Disclosed is a carbon fiber having a random structure in at least a part of a cross-sectional structure, a uniform pulverized product obtained by pulverization, and excellent heat dissipation characteristics. In producing a carbon fiber precursor from a mesophase pitch by a melt blow method, the melt viscosity of the mesophase pitch in the capillary is 0.1 to 3 Pa ยท s, the flow rate is 0.15 to 1.50 m / s, The infusibilizing treatment and the firing treatment are performed on the obtained carbon fiber precursor. [Selection] Figure 1 |
isCitedBy | http://rdf.ncbi.nlm.nih.gov/pubchem/patent/WO-2010071226-A1 |
priorityDate | 2007-05-21-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type | http://data.epo.org/linked-data/def/patent/Publication |
Incoming Links
Total number of triples: 20.