http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2008284757-A
Outgoing Links
Predicate | Object |
---|---|
assignee | http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_c3a9faef4b414dd2b3ff22bf3ca4fd82 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B32B27-36 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B32B27-32 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/G09F3-04 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B65D65-40 |
filingDate | 2007-05-16-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor | http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_12bd32640159781e454a0ec895be3bf8 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_437b3a12f5a46cb9438cd22556171210 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_b0bfa38a024b54bc844c9b7db920bc92 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_fff1e450e2b79254bc35196758bde74a |
publicationDate | 2008-11-27-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | JP-2008284757-A |
titleOfInvention | Shrink film and shrink label |
abstract | Disclosed is a shrink film that exhibits high interlayer strength among laminated shrink films of different polymers of polyolefin resin and polyester resin. A shrink film of the present invention comprises a surface layer (A layer) composed of a resin composition A mainly composed of an amorphous polyester resin, and 35% by weight of a polyolefin resin having a reactive functional group. An intermediate layer (B layer) comprising a resin composition B containing a polyolefin-based resin as a main component and a center layer (C layer comprising a resin composition C containing a polyolefin-based resin as a main component. ) Are laminated in the order of A layer / B layer / C layer / B layer / A layer without interposing other layers, and each resin of the resin compositions A to C The absolute value of the difference in melt viscosity at 220 ° C. between the compositions is 300 Pa · s or less, and the absolute value of the difference in the slope of the temperature-melt viscosity line at 200 to 240 ° C. is 7 Pa · s / ° C. or less. It is characterized by. [Selection figure] None |
isCitedBy | http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2013226711-A |
priorityDate | 2007-05-16-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type | http://data.epo.org/linked-data/def/patent/Publication |
Incoming Links
Total number of triples: 113.