http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2008276006-A
Outgoing Links
Predicate | Object |
---|---|
assignee | http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_1a01de6634586136b39f82c1fba1be98 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/G02F1-17 |
filingDate | 2007-05-01-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor | http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_e78538707c2c6dd318d852d07ab85545 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_627da366b2ec6930c1db7be82f340165 |
publicationDate | 2008-11-13-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | JP-2008276006-A |
titleOfInvention | Magnetic display sheet |
abstract | A magnetic display sheet having a stable dispersibility of reddish brown γ-iron oxide and capable of displaying clear reddish brown characters and images with good contrast. A magnetic display sheet of the present invention has a transparent sheet for writing, a solid dispersion layer having a microcapsule containing a dispersion containing a white pigment and reddish brown γ-iron oxide, and a support in this order. A product of the specific surface area of the reddish brown γ-iron oxide and the viscosity (25 ° C.) of the dispersion is γ-iron oxide and the dispersion in a range of 240 to 680. Individually, when the specific surface area of the reddish brown γ-iron oxide and the viscosity (25 ° C.) of the dispersion is 14 m 2 / g, the viscosity (25 ° C.) is 44 mPa · s or less. When the specific surface area is 20 m 2 / g or less, the viscosity (25 ° C.) is 33 mPa · s or less, or when the specific surface area is 24 m 2 / g or less, the viscosity (25 ° C.) is 28 mPa · s or less. One of the selected. [Selection] Figure 1 |
priorityDate | 2007-05-01-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type | http://data.epo.org/linked-data/def/patent/Publication |
Incoming Links
Total number of triples: 54.