http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2008272578-A
Outgoing Links
Predicate | Object |
---|---|
assignee | http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_25afcb7bf2c0d839bb9118680e60e1ae http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_605e09fc2a90997ff063dc52a13bc6db |
classificationCPCAdditional | http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/Y02W30-78 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/Y02W30-58 |
classificationIPCAdditional | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/A62D101-41 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/A62D101-28 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/A62D101-43 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/A62D101-22 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B09B3-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/A62D3-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/A62D3-40 |
filingDate | 2007-02-01-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor | http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_841f3c9e5a48b8069ec9cdcd2b183acb http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_ee8f7793077a5920f571bb5dbaf142fc |
publicationDate | 2008-11-13-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | JP-2008272578-A |
titleOfInvention | Method for low-temperature detoxification treatment of hazardous waste containing hazardous substances and method for producing recycled materials |
abstract | The present invention provides an asbestos detoxification method that recovers asbestos waste while preventing asbestos from being scattered, decomposes the waste with low energy, and recycles a detoxified fired product. SOLUTION: 0.05 to 1 part by weight of an alkali metal hydroxide, 0.05 to 1 part by weight per 1 part by weight of a hazardous waste crushed material obtained by crushing and crushing hazardous waste containing harmful substances 1 part by weight of an alkaline earth metal hydroxide, 0.5 to 20 parts by weight of a reducing substance and 0.1 to 5 parts by weight of water are kneaded to form a kneaded material, and the kneaded material is shaped. , A low-temperature detoxification method for hazardous waste, which is produced by firing at a temperature of 700 to 1000 ° C. for 10 to 60 minutes to produce a detoxified fired product. [Selection] Figure 1 |
isCitedBy | http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2014237069-A http://rdf.ncbi.nlm.nih.gov/pubchem/patent/CN-103978013-A |
priorityDate | 2007-02-01-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type | http://data.epo.org/linked-data/def/patent/Publication |
Incoming Links
Total number of triples: 56.