http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2008266624-A
Outgoing Links
Predicate | Object |
---|---|
assignee | http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_24aca9ded2638ea793d05360dde7a4a0 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08F10-00 |
filingDate | 2008-03-25-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor | http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_a0205953d8ef4cc98773d7a98474de41 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_076a4236f8cc83189dda29901d6ca122 |
publicationDate | 2008-11-06-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | JP-2008266624-A |
titleOfInvention | Low crystalline or amorphous modified olefin resin |
abstract | To provide a low crystalline or amorphous modified olefin resin having excellent elongation characteristics, scratch resistance and molding processability. A low crystalline or amorphous modified olefin resin satisfying all of the following (i) to (v). (I) It contains monomer units derived from at least two olefins selected from the group consisting of ethylene, propylene and olefins having 4 to 20 carbon atoms, and the content of monomer units derived from ethylene is 60. Mol% or less (however, the entire low-crystalline or amorphous modified olefin resin is 100 mol%) (Ii) In the differential scanning calorimetry according to JIS K7122, the heat of fusion of crystals obtained by measurement in the range of −50 ° C. to 200 ° C. is 30 J / g or less (iii) The branching index is less than 1 (iv) The molecular weight distribution is 1 .5-3 (V) MFR 0.1-30g / 10min [Selection figure] None |