http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2008260957-A
Outgoing Links
Predicate | Object |
---|---|
assignee | http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_d1a84d1b7b5e81f099ec2d4d905a74fc |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08L53-02 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08K5-14 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08L91-00 |
filingDate | 2008-08-04-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor | http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_e3f9a8716215a8861e7005ba9b95d5fc |
publicationDate | 2008-10-30-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | JP-2008260957-A |
titleOfInvention | Thermoplastic elastomer composition and molded body |
abstract | PROBLEM TO BE SOLVED: To form a gel having a hardness of 40 A or less at room temperature, which can be easily manufactured and molded, has excellent moisture retention, has little oil bleed feeling, and has a smooth surface feeling, such as polyethylene and polyurethane. Disclosed are a thermoplastic elastomer composition excellent in adhesion to a film, hardly torn even under high temperature and high pressure, excellent in oil resistance and compression set, and a molded product thereof. (A) 100 parts by weight of a softener for non-aromatic hydrocarbon rubber, (b) 3 to 110 parts by weight of a hydrogenated and / or partially hydrogenated block copolymer (c) 0.1 of a surfactant A thermoplastic elastomer composition containing -30 parts by weight and (d) 0.01-10 parts by weight of an organic peroxide, and a molded product thereof. [Selection figure] None |