http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2008222842-A
Outgoing Links
Predicate | Object |
---|---|
assignee | http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_9317c0cce712dbf1a1a2252d652451f9 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B05D5-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C09D5-16 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C09D1-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B01J35-02 |
filingDate | 2007-03-12-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor | http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_8807aa5ba7419bf4620e7a4a5d404306 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_6aa47c044910c5d3b88b483df43f1648 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_11e3e84ce4e436c9cafcc45b4abba757 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_79cca05115cee2c91bcd810e41cde5d7 |
publicationDate | 2008-09-25-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | JP-2008222842-A |
titleOfInvention | Photocatalytic coating film forming coating agent and photocatalytic coating film forming method |
abstract | Provided are a photocatalyst film exhibiting photocatalytic activity under visible light and weak ultraviolet light and having high durability, a coating agent used for forming a photocatalyst film, and a photocatalyst film forming method. First, a coating agent containing scaly titanium oxide fine particles 5, a sulfur-containing compound, and a titanium alkoxide 7 as a binder is prepared. Next, the photocatalyst coating film 1 is formed by apply | coating the coating agent to the surface of the base material 3 by a spin coat method, drying, and heating to the temperature of 400-600 degreeC. [Selection] Figure 1 |
isCitedBy | http://rdf.ncbi.nlm.nih.gov/pubchem/patent/WO-2022181210-A1 |
priorityDate | 2007-03-12-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type | http://data.epo.org/linked-data/def/patent/Publication |
Incoming Links
Total number of triples: 88.