http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2008203785-A
Outgoing Links
Predicate | Object |
---|---|
assignee | http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_4af0df9a26ff4aafde7285cbd8eb12f4 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/G03G21-10 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/G03G9-08 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/G03G9-113 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/G03G9-087 |
filingDate | 2007-02-22-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor | http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_3a23de9f6dbdac085a6470dc926c99b4 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_03b931167c849785b73114f5d11ce0f2 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_97291845e39df9803ba0cd556e8b6053 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_92bd74e89eb80a99599ca4a429f546a1 |
publicationDate | 2008-09-04-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | JP-2008203785-A |
titleOfInvention | Toner for electrostatic charge development and method for producing the same, developer for electrostatic charge development, and image forming apparatus |
abstract | Production of an electrostatic charge developing toner and an electrostatic charge developing toner excellent in blade cleaning properties in an electrophotographic process by controlling the structure of a crystalline substance on the toner surface and controlling the toner surface friction coefficient The present invention provides a method, a developer for developing an electrostatic charge, and an image forming apparatus. An electrostatic charge developing toner includes a crystalline polyester resin 12 and a release agent 10 and has a surface friction coefficient μ of 0.21 to 0.45 and is ruthenium-stained. When there is a structure 100 in which the crystalline resin polyester resin 12 is in contact with the release agent 10 on the cross section of the toner, the cross-sectional area of the structure 100 is A, and the cross-sectional area of the release agent 10 alone is B 60 ≦ 100 × A / (A + B) ≦ 100, and the surface of the toner has a hydrophobized metal oxide. [Selection] Figure 2 |
isCitedBy | http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2018031986-A http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2016218119-A http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-9213250-B2 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2018018069-A |
priorityDate | 2007-02-22-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type | http://data.epo.org/linked-data/def/patent/Publication |
Incoming Links
Total number of triples: 358.