http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2008195775-A
Outgoing Links
Predicate | Object |
---|---|
assignee | http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_95136e4276343dbae035a63330dabfc7 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08J5-18 |
filingDate | 2007-02-09-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor | http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_b81a2f50cb5465523e084d6548eff515 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_98b37d2d9e74833deaf6b9b380d67cd4 |
publicationDate | 2008-08-28-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | JP-2008195775-A |
titleOfInvention | Polyester film |
abstract | PROBLEM TO BE SOLVED: To provide a film by forming a polyester having good crystallinity and a low melting point. SOLUTION: A film formed by forming a polyester, wherein the polyester contains terephthalic acid as a dicarboxylic acid component, 1,6-hexanediol and ethylene glycol as diol components, and 50% of all diol components. A film formed by forming a polyester having a DSC curve satisfying the following formula (1) whose mol% or more is 1,6-hexanediol, melting point is 100 to 150 ° C. . b / a ≧ 0.02 mW / mg · ° C. (1) [Selection figure] None |