http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2008179043-A
Outgoing Links
Predicate | Object |
---|---|
assignee | http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_5b354acbffbe119a27ccd31d99fdd8df |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B60R13-02 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B32B27-30 |
filingDate | 2007-01-24-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor | http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_e0aec455a3892ffd963f9b7d3c23169f http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_3ae1a97df72972e1c97904bac6f2a127 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_77c433b04df62113d8c198fec54347a0 |
publicationDate | 2008-08-07-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | JP-2008179043-A |
titleOfInvention | Multi-layer film for decoration |
abstract | [Problem] To provide a multilayer film for decoration having excellent chemical resistance and transparency. SOLUTION: An acrylic resin is used as a base material (1), a rubber-like polymer, an aromatic vinyl monomer, a (meth) acrylic acid ester monomer, or other vinyl monomers copolymerizable therewith. A) the weight average particle diameter of the rubbery polymer is 0.05 to 0.15 μm, and b) the difference in refractive index between the acetone insoluble part and the soluble part in the composition is 0. A multilayer film for decoration, which is formed by laminating a rubber-reinforced styrene resin composition of less than 0.02 as a surface layer (2). [Selection figure] None |
isCitedBy | http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2016509112-A http://rdf.ncbi.nlm.nih.gov/pubchem/patent/CN-113226758-B http://rdf.ncbi.nlm.nih.gov/pubchem/patent/CN-113226758-A |
priorityDate | 2007-01-24-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type | http://data.epo.org/linked-data/def/patent/Publication |
Incoming Links
Total number of triples: 61.