http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2008169236-A
Outgoing Links
Predicate | Object |
---|---|
assignee | http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_ad2cd796f8c4dcb425ddcc68707d3444 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08G73-10 |
filingDate | 2007-01-09-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor | http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_666680f5646defad712fcf627b36cc16 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_7b994a9d0e27dfe5ee5ea5b24920afde http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_b266c7dd60edeaeb6c38b292f82f60da |
publicationDate | 2008-07-24-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | JP-2008169236-A |
titleOfInvention | Non-thermoplastic polyimide non-planar molded product and method for producing the same |
abstract | PROBLEM TO BE SOLVED: To obtain a thin, non-planar molded product of non-thermoplastic polyimide which is free from adverse effects due to solvent volatilization and has excellent heat resistance when formed into a molded product with imidization and molding. I will provide a. SOLUTION: A non-thermoplastic polyimide non-planar molded product having an aromatic tetracarboxylic acid residue and an aromatic diamine residue in the main chain, a thickness of 1 to 50 μm, and a heating volatile content of 5 A method for producing a non-thermoplastic polyimide non-planar molded product in which a polyamic acid film of less than mass% is molded and then heated to an imidization temperature or higher to be converted into polyimide. [Selection figure] None |
isCitedBy | http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2010509390-A |
priorityDate | 2007-01-09-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type | http://data.epo.org/linked-data/def/patent/Publication |
Incoming Links
Total number of triples: 164.