http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2008168597-A
Outgoing Links
Predicate | Object |
---|---|
assignee | http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_1ab0947d66370d3a49ea2b47eb74050c |
classificationCPCAdditional | http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/Y02E60-50 |
classificationIPCAdditional | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B29K101-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B29L7-00 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08J5-18 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/H01M8-02 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B29C41-12 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/H01M8-10 |
filingDate | 2007-01-15-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor | http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_c9eaa7d167910f1c11dc8594c5d8f1ed http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_7cf5db2ef082f2571f32b6dab32a5cab |
publicationDate | 2008-07-24-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | JP-2008168597-A |
titleOfInvention | Method for forming polymer thin film and polymer thin film |
abstract | PROBLEM TO BE SOLVED: To provide a film forming method for a polymer thin film which can be easily formed even if it is a thin film of less than 10 μm and the surface flatness is ensured. A polymer solution in which a polymer is dissolved in a solvent is applied to a flat substrate surface and dried near the saturated vapor pressure of the solvent to produce a polymer thin film. The solvent is preferably a hydrophilic organic solvent having a surface tension smaller than that of water or an aqueous solution thereof, and is preferably dried in the vicinity of the saturated vapor pressure over 2 hours or more. [Selection] Figure 1 |
priorityDate | 2007-01-15-04:00^^<http://www.w3.org/2001/XMLSchema#date> |