http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2008156408-A
Outgoing Links
Predicate | Object |
---|---|
assignee | http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_24aca9ded2638ea793d05360dde7a4a0 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08J3-21 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08L23-08 |
filingDate | 2006-12-21-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor | http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_32392dae0672843cfaf25af598dca073 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_e0611e99593827390e23806feed486d4 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_e89020df9a6bbf8202390856e7eb2165 |
publicationDate | 2008-07-10-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | JP-2008156408-A |
titleOfInvention | Process for producing olefinic thermoplastic elastomer |
abstract | Provided is a method for efficiently producing an olefinic thermoplastic elastomer as a material for producing a molded article having a good appearance. An olefin copolymer rubber (A), a volatile organic solvent (B), and an olefin resin (C) obtained by polymerizing ethylene, an α-olefin having 3 to 20 carbon atoms, and a non-conjugated polyene. The volatile organic solvent (B) is removed while kneading in an extruder, then the crosslinking agent (D) is added, and the volatile organic solvent (B) is removed while kneading in an extruder. To produce an olefinic thermoplastic elastomer. [Selection figure] None |
isCitedBy | http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2010523809-A http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-9434835-B2 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2008174732-A http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2013057060-A |
priorityDate | 2006-12-21-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type | http://data.epo.org/linked-data/def/patent/Publication |
Incoming Links
Total number of triples: 124.