http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2008121024-A
Outgoing Links
Predicate | Object |
---|---|
assignee | http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_e000ed5aabdb2248a1e5a269ab0e310e |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08G77-48 |
filingDate | 2008-01-31-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor | http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_3491a0de94724668bcfbc5ded351b12d http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_8b8de6f2f53c2f43eeb394c9e4bdcb21 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_0968a561b88489be609215a17d3b0a0d |
publicationDate | 2008-05-29-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | JP-2008121024-A |
titleOfInvention | Granular silicone cured product and method for producing the same |
abstract | PROBLEM TO BE SOLVED: To provide a granular silicone cured product having special viscoelasticity and good tactile sensation, and a method for producing the same. (A) A polydiorganosiloxane having at least two silicon-bonded alkenyl groups in one molecule, (B) an average unit formula: (R 3 SiO 1/2 ) x (SiO 4/2 ) 1.0 ( In which R is the same or different monovalent hydrocarbon group, provided that at least one R in one molecule is an alkenyl group, and x is a number from 0.6 to 4.0. And (C) a polyorganosiloxane having at least two silicon-bonded hydrogen atoms in one molecule, and (D) a mean catalyst having a mean particle size of 0.1 to 0.1. The method for producing a granular silicone cured product according to claim 1, wherein the cured granular silicone product is 500 μm, the components (A) to (C) are dispersed in water with an emulsifier and cured with the component (D). [Selection figure] None |