http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2008096300-A
Outgoing Links
Predicate | Object |
---|---|
assignee | http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_44ff3005508304394801e265e503b811 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/G02B1-10 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/G01N17-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/G01N19-04 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/G02B1-115 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/G02B1-14 |
filingDate | 2006-10-12-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor | http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_2f6d9c94ec53bdd3de2e41e8813b27f1 |
publicationDate | 2008-04-24-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | JP-2008096300-A |
titleOfInvention | Test condition determination method and test method for adhesion performance of titanium-based hard coat with lens base material |
abstract | The present invention provides a method capable of evaluating a temporal decrease in the adhesion of a titanium hard hard coat film to a plastic lens substrate. A lens base material of a titanium-based hard coat film provided on a plastic lens base material by testing a test lens subjected to an exposure process in which exposure to ultraviolet irradiation and exposure to a dew condensation state are repeated. A method for determining the conditions of exposure treatment in a method for testing adhesion to a body. (1) A lens using a plastic lens substrate of the same quality as the lens to be examined is exposed to xenon light irradiation, and the reference ΔYI value before and after the xenon light irradiation exposure of the obtained lens changed to yellow is obtained. ) Conditions for the exposure treatment are set such that the lens subjected to the exposure treatment exhibits a reference ΔYI value. The test lens is subjected to the exposure treatment under the conditions determined by this method, and the cross-hatch test is performed on the lens surface of the test lens subjected to the exposure treatment to evaluate the adhesion performance of the hard coat film to the lens substrate. . [Selection figure] None |
isCitedBy | http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2012032241-A http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-7262198-B2 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2020056831-A http://rdf.ncbi.nlm.nih.gov/pubchem/patent/CN-112394029-A http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2012132843-A http://rdf.ncbi.nlm.nih.gov/pubchem/patent/WO-2020067465-A1 |
priorityDate | 2006-10-12-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type | http://data.epo.org/linked-data/def/patent/Publication |
Incoming Links
Total number of triples: 161.