http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2008093616-A
Outgoing Links
Predicate | Object |
---|---|
assignee | http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_646018b7183a929bbb6e26dcdb62a8da |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B05D7-14 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B05D1-36 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B05D5-06 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B05D7-24 |
filingDate | 2006-10-16-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor | http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_d87a34e6c2a9ed3a273f5ad12ebf1da8 |
publicationDate | 2008-04-24-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | JP-2008093616-A |
titleOfInvention | Method for forming coating film on metal light alloy wheel |
abstract | PROBLEM TO BE SOLVED: To reduce the yield without causing appearance defects even when a metallic layer is formed by making the powder electrostatic coating layer sufficiently thick so that the unevenness of the casting surface is eliminated in appearance. A method for forming a coating film on an alloy wheel is provided. A method of forming a coating film of a metal light alloy wheel, in which a powder coating is blown from the back side of the design surface of the light alloy wheel base to form a layer by electrostatic coating on at least a part of the surface side of the design surface. It has the process of forming, and the process of forming a metallic layer in the upper layer side rather than the said electrostatic coating layer, It is characterized by the above-mentioned. [Selection] Figure 1 |
isCitedBy | http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2018118368-A http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2011235593-A |
priorityDate | 2006-10-16-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type | http://data.epo.org/linked-data/def/patent/Publication |
Incoming Links
Total number of triples: 25.