http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2008071536-A
Outgoing Links
Predicate | Object |
---|---|
assignee | http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_9df90d7822cc480ce12c480f4089e229 http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_c186e9ae8cafab5df5c8d80cfa7b0fa1 |
classificationCPCAdditional | http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/Y02E60-10 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/H01M4-36 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/H01M4-32 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/H01M4-52 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/H01M4-30 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/H01M4-80 |
filingDate | 2006-09-12-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor | http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_3e12354455a2ad0fbc4b1b932f68c5ab http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_79d16d80ad4d8d73f4aa6bce54d427db http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_7d73de539e39ec95590dc96cc1fb766a http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_16073d9bb7f9b6840a94c2ef49098330 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_ddab9b8a02d3b6329c9829c3cd6579c7 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_f8c9be88b77cfaa78524f6065ae465be |
publicationDate | 2008-03-27-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | JP-2008071536-A |
titleOfInvention | Nickel electrode for alkaline battery and method for producing the same |
abstract | A nickel electrode for an alkaline battery having excellent charge / discharge cycle characteristics and a method for producing the same are provided. A nickel electrode according to the present invention is an electrode base material in which a non-woven fabric in which most of fibers are oriented in one direction is subjected to nickel plating to produce a current collector, and the current collector is filled with an active material. Is roll-pressed along the fiber direction of the nonwoven fabric. In the nickel electrode of the present invention, when the electrode base material is roll-pressed, the elongation of the nickel electrode is suppressed, and the reduction rate of the thickness of the nickel electrode is increased. By increasing the thickness reduction rate, the packing density of the active material of the nickel electrode is increased and the expansion of the nickel electrode is suppressed. When this nickel electrode is used in a battery, the swelling can be effectively suppressed. it can. [Selection] Figure 1 |
isCitedBy | http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2016501425-A |