http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2008067444-A
Outgoing Links
Predicate | Object |
---|---|
assignee | http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_6f33d2546036ff94c827377f52deeb35 |
classificationCPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/H02N11-006 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/F03G7-005 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C23C18-31 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C23C18-16 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/H02N11-00 |
filingDate | 2006-09-05-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor | http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_8a92773fd0ca488ba7281f084f9bf32a |
publicationDate | 2008-03-21-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | JP-2008067444-A |
titleOfInvention | Method for filling polymer actuator element with electrolyte, method for controlling elastic modulus of polymer actuator element, and method for manufacturing polymer actuator element |
abstract | Disclosed is a method for filling a polymer actuator element with an electrolyte solution that can be easily filled with an electrolyte solution containing a liquid nonionic compound at room temperature and normal pressure. Moreover, the elastic modulus control method of the polymer actuator element which can adjust easily the elasticity modulus of the polymer actuator element which has the electrolyte solution containing a liquid nonionic compound under normal temperature normal pressure is provided. Furthermore, the present invention provides a simple method for producing a polymer actuator element having an electrolytic solution containing a nonionic compound that is liquid at normal temperature and pressure. A method for filling an electrolyte solution of a polymer actuator element including a polymer composite provided with a metal electrode on a polymer electrolyte, wherein the polymer composite is a liquid nonionic compound at room temperature and normal pressure. And a second step of immersing the polymer composite in a solution obtained by further adding an electrolyte to the solution. Method. [Selection figure] None |
isCitedBy | http://rdf.ncbi.nlm.nih.gov/pubchem/patent/WO-2011046161-A1 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2010016969-A http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2010041878-A http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2011087387-A http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2010041876-A |
priorityDate | 2006-09-05-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type | http://data.epo.org/linked-data/def/patent/Publication |
Incoming Links
Total number of triples: 99.