http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2008062182-A
Outgoing Links
Predicate | Object |
---|---|
assignee | http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_c2d6cc21bc7bce139ac89fd102222f74 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C09D7-12 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B05D1-40 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C09D191-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C09D5-00 |
filingDate | 2006-09-07-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor | http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_0119b995439bce2d244b73304b93855d http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_9d4889e8e1e3454e643adc1ec1c83969 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_9041c895b43601d1b02f17a7dcf16159 |
publicationDate | 2008-03-21-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | JP-2008062182-A |
titleOfInvention | Method for forming a highly water-repellent surface |
abstract | 【Task】 Provided is a method for easily forming a highly water-repellent surface having a fine uneven structure. [Solution] Mass of water repellent fine particle metal oxide dispersion type compound containing a water repellent surface treated fine particle metal oxide having a primary particle size in the range of 10 nm to 50 nm, a drying oil and a volatile solvent, and excluding the volatile solvent. The fine particle metal oxide dispersion type compound in which the compounding mass of the water-repellent surface-treated fine particle metal oxide is in the range of 60 to 80% by mass is applied to the substrate surface using a spin coating method. Method for forming a highly water-repellent surface. [Selection figure] None |
isCitedBy | http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-11525779-B2 |
priorityDate | 2006-09-07-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type | http://data.epo.org/linked-data/def/patent/Publication |
Incoming Links
Total number of triples: 79.