http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2008038052-A
Outgoing Links
Predicate | Object |
---|---|
assignee | http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_24aca9ded2638ea793d05360dde7a4a0 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08L23-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08K3-34 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08L71-12 |
filingDate | 2006-08-08-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor | http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_8656d853aa413db00bf294252c81a543 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_5d23bd800c7622fe4a54c8078c6baeca |
publicationDate | 2008-02-21-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | JP-2008038052-A |
titleOfInvention | Thermoplastic resin composition |
abstract | Disclosed are a thermoplastic fat composition having excellent mechanical properties and excellent flame retardancy, and a resin-coated product formed by coating the same. SOLUTION: A polyolefin resin (component (A)), a thermoplastic resin (component (B)) having an oxygen index of 24 or more, and a plate-like filler having a weight average particle size of 3 to 10 μm determined by a laser diffraction method. A thermoplastic resin composition containing (component (C)), wherein the weight ratio ((A) / (B)) of component (A) and component (B) is 80/20 to 20 / 80, the content of the component (C) is 5 to 50 parts by weight with respect to 100 parts by weight of the total weight of the component (A) and the component (B), and the component (C) is the component (B ) And a resin-coated product obtained by coating the thermoplastic resin composition in which component (A) forms a continuous phase. [Selection figure] None |
isCitedBy | http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2018035218-A |
priorityDate | 2006-08-08-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type | http://data.epo.org/linked-data/def/patent/Publication |
Incoming Links
Total number of triples: 122.