http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2008037999-A
Outgoing Links
Predicate | Object |
---|---|
assignee | http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_1374dd16777534b65ad4422333245af8 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08G69-26 |
filingDate | 2006-08-04-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor | http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_dce23587366c33dacbe3b0134191aada http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_e3563b6617f3a1eeaeaf91e3572d8452 |
publicationDate | 2008-02-21-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | JP-2008037999-A |
titleOfInvention | Molding dope |
abstract | [Problem] To provide a dope for molding that can be used as a stock solution for molding which is useful in producing a polyamide molded article having excellent heat resistance and mechanical properties, particularly fibers, films and pulp-like particles. The following formula (I) [Chemical 1] And the following formula (II) [Chemical 2] The copolymerization molar ratio (II) / (I) of the repeating units of the above formulas (I) and (II) is 1 ≦ (II) / (I) ≦ 100. The dope for shaping | molding containing the polymer and solvent which are in the range of this, and the density | concentration of a polymer is 5 weight% or more. [Selection figure] None |
isCitedBy | http://rdf.ncbi.nlm.nih.gov/pubchem/patent/CN-116470126-A |
priorityDate | 2006-08-04-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type | http://data.epo.org/linked-data/def/patent/Publication |
Incoming Links
Total number of triples: 94.