http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2008037912-A
Outgoing Links
Predicate | Object |
---|---|
assignee | http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_67f2bb9a79bd8433343ae221f81551cf |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08J7-04 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08J7-12 |
filingDate | 2006-08-02-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor | http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_36688bf0856f9ff6f0e49300d4508e86 |
publicationDate | 2008-02-21-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | JP-2008037912-A |
titleOfInvention | Resin substrate and surface modification method thereof |
abstract | The present invention provides a method for modifying a film surface that is not easily soiled or scratched, and a method for modifying a permanent surface that maintains initial performance even after washing and cleaning with water or a solvent. A surface modification of a resin substrate characterized by immobilizing a fluorine compound represented by the following general formula (1) on a resin substrate with a crosslinking agent having an isocyanate group protected by a protecting group. Method. [Chemical 1] In the formula, Rf is a group containing a fluorine atom having 1 to 30 carbon atoms, X is a divalent linking group, A is a divalent linking group containing a polyalkylene oxide chain, and m and n are 0 or 1. [Selection figure] None |
isCitedBy | http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-8739976-B2 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/KR-101319085-B1 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/WO-2011030725-A1 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-5621775-B2 |
priorityDate | 2006-08-02-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type | http://data.epo.org/linked-data/def/patent/Publication |
Incoming Links
Total number of triples: 86.