http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2008013770-A
Outgoing Links
Predicate | Object |
---|---|
assignee | http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_6bc6166c47b8fba20bdc2327894cc0a0 |
classificationCPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08F240-00 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C09J7-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08F240-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C09J109-06 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C09J157-02 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C09J153-02 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/G09F3-10 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C09J123-08 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C09J131-04 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08F32-02 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C09J125-10 |
filingDate | 2007-07-30-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor | http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_fdebd62a0f955678b301715ed7ea94b1 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_03d5001730ff24763c90114e3cca2ea0 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_35aea9a93b5aa2a9e0a8ac7c83ba59ae |
publicationDate | 2008-01-24-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | JP-2008013770-A |
titleOfInvention | Oil-based aliphatic resin, method for controlling softening point and molecular weight of the resin, and pressure-sensitive hot melt adhesive containing the resin |
abstract | An aliphatic resin useful for imparting tackiness with controlled softening point and molecular weight, And a method for producing the same, and a pressure-sensitive adhesive composition containing these resins. The present invention relates to a) a ring and ball (R & B) softening point of 75 to 110 ° C .; b) Weight average molecular weight (Mw) is 1000-2600 Dalton, z average molecular weight (Mz) Is 1900-5000 Dalton, and Mw / Mn is 2.0 or less; c) 1 H—N It provides a petroleum-based aliphatic resin having an aromatic proton level of 1.5% or less relative to the total protons measured by MR; and d) a mixed methylcyclohexaneaniline cloud point (MMAP) of 90 ° C. or less. . The resin according to the present invention is characterized by having a very large number of cyclic structures. Furthermore, in the method of independently controlling the R & B softening point and molecular weight of an aliphatic resin composition during its production by polymerizing a petroleum based feedstock, the amount of the cyclic structure of the resin is increased. Describes how to do this. [Selection figure] None |
isCitedBy | http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2015513321-A http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2014198806-A |
priorityDate | 1996-03-06-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type | http://data.epo.org/linked-data/def/patent/Publication |
Incoming Links
Total number of triples: 81.