http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2008013748-A
Outgoing Links
Predicate | Object |
---|---|
assignee | http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_7f9af914ed2fb00cd4f1b8b1a28964e4 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08F6-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08F20-06 |
filingDate | 2007-04-18-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor | http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_c7f4dc905eea732ea5f61615f11f8b27 |
publicationDate | 2008-01-24-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | JP-2008013748-A |
titleOfInvention | Method for producing (meth) acrylic acid (salt) water-soluble polymer |
abstract | A (meth) acrylic acid (salt) water-soluble polymer having a high molecular weight and a high molecular weight (meth) acrylic acid (salt) water-soluble polymer with sufficiently reduced insoluble content. A manufacturing method is provided. A method for producing a (meth) acrylic acid (salt) -based water-soluble polymer by drying a (meth) acrylic acid (salt) -based water-soluble polymer-containing gel, wherein the production method comprises a dew point. (Meth) acrylic acid (salt) -based aqueous solution comprising a step of drying such that hot air having a temperature of 70 ° C. or lower and a temperature of 160 to 230 ° C. passes through the hydrogel gap at a linear velocity of 0.1 m / s or higher. For producing a conductive polymer. [Selection figure] None |
isCitedBy | http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2016532001-A http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2010155901-A |
priorityDate | 2006-06-07-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type | http://data.epo.org/linked-data/def/patent/Publication |
Incoming Links
Total number of triples: 142.